e.t.d. 150® Properties


ASTM A311 Class B

Tensile Strength

** 150,000 psi

Yield Strength (.2% offset)

130,000 psi

Machining Characteristics

75% of 1212

Elongation

5% Min.

Reduction of Area

20% Min.

Rockwell C Hardness

** 32 Min.

Brinell Hardness

** 302 Min.

Micro-Structure

Ferritic fine grain and bainite/pearlite

Fine grain size 5 – 8

Size Range

7/16″ rounds through 3 1/2″

Length

11′ / 13′

Any Custom Lengths

Finish

Standard “As Drawn” finish is smooth, accurate, and dark in color

Ground & Polished finish provides close tolerances, high accuracies and bright surface.

Rounds Only

Example of Use

Parts you are now heat treating from Rc30 to Rc36.

Tolerances

(Tolerances, in decimals of an inch, provide for undersize variation only)

Rounds:

* E.T.D. 150® contains additives for improving machinability. These may be Tellurium, Selenium, Sulfur (.06 max), or others, separately or in combination.